| Sign In | Join Free | My benadorassociates.com |
|
Brand Name : HUAYE
Certification : BV. SGS
Place of Origin : China
Product name : Nickel Bar
Material : inconel 625
Ni (Min) : 68%
Resistance (μΩ.m) : standard
Powder Or Not : Not Powder
Ultimate Strength (≥ : MPa): 965
Elongation (≥ %) : 30
Application : widely, in air plane, oil
| Place of Origin: | Jiangsu, China |
| Type: | Nickel Bar |
| Application: | widely, in air plane, oil |
| Grade: | inconel 625 |
| Ni (Min): | 68% |
| Resistance (μΩ.m): | standard |
| Powder Or Not: | Not Powder |
| Ultimate Strength (≥ MPa): | 965 |
| Elongation (≥ %): | 30 |
| Model Number: | inconel 625 |

|
|
Superalloy Nickel Alloy Inconel Flat Bar 600 625 718 725 750 907 Images |